Objective

  • Make 40% beads

Description

  • Make 40% Beads
  • Same procedure as yesterday with these amounts:
  • 1.25g PVOH, 27 mL bentonite solution, 15mL HCl, 13mL water
  • Freeze Dry
  • Put beads in -80°C freezer for 40 mins.
  • Put frozen beads in freeze dryer until Wednesday.

Data

  • Add data and results here...

Notes

This area is for any observations or conclusions that you would like to note.