Objectives
- Analyze the 20% Bentonite beads and 30% powder Bentonite beads via UV VIS
- Synthesize 30% Bentonite beads using solution instead of powder
- Prepare plastic column
Procedure
- Analysis of the 20% Bentonite beads and 30% powder Bentonite beads via UV VIS:
- These beads were analyzed using the same procedure as the 10% bentonite beads, from the 28th.
- Synthesis of 30% Bentonite beads
- The synthesis of 30% bentonite beads was prepared using the same procedure from the 21st with the only difference being the use of 25mL of 3% wt Bentonite solution and 3.5mL of water.
- Preparation of the plastic column
- Preparation of the plastic column was carried out using the same procedure that was used on the 16th.
|