Making nitrocellulose coverslips
From OpenWetWare
Jump to navigationJump to search
Making Nitrocellulose Coverslips
1. Make bead/Triton mixture: 1 μL beads + 199 μL 0.2% Triton X-100
2. Spread 7.5 μL on each slide
3. Allow coverslips to dry
4. Dip coverslips in 0.1% collodion in amyl acetate
Recipes
| 2.5 mL 0.2% Triton | |
|---|---|
| 25% Triton X-100 | 20 μL |
| sterile water | 2.5 mL |
| 20 mL 0.1% Collodion | |
|---|---|
| 2% collodion in amyl acetate | 1 mL |
| Amyl acetate | 19 mL |