User:Sarah Burkhard/Notebook/CHEM 481 Polymers/2016/09/21
From OpenWetWare
Project name | Main project page Previous entry Next entry |
Tasklist
Protocol30 % clay solution beads were prepared with the following volumes:
Except for the solution, we followed | this protocol ObservationsThe beads looked finer and smaller than previous beads. After removing ethylacetate, some of the beads show to have clumped, both for 30 and for 40 percent clay. Additionally, the beads seemed to have a lower density of water: now, the beads form the upper phase of the water - beads layers. |