Preparation of Au/Zn core-shell NP

  • 1 mL AuNP (His/NH4OH) + 1mL His + 1 mL NH4OH + 1 mL ZnAc2 + 6 mL H2O
  • 1 mL AuNP (His/NaOH) + 1mL His + 1 mL NaOH + 1 mL ZnAc2 + 6 mL H2O
  • 1 mL AuNP (Cys/NH4OH) + 1mL Cys + 1 mL NH4OH + 1 mL ZnAc2 + 6 mL H2O
  • 1 mL AuNP (Cys/NaOH) + 1mL Cys + 1 mL NaOH + 1 mL ZnAc2 + 6 mL H2O
  • Used same stock solutions prepared yesterday
  • Samples placed in 80 C oven