==February 20, 2015== | ==February 20, 2015== | ||
*Get pXRD data > analysis | *Get pXRD data > analysis | ||
**Running molding clays | |||
*Rehydrate PVA-Alg-NaMT no citric acid beads in 2 ppm Malachite Green | *Rehydrate PVA-Alg-NaMT no citric acid beads in 2 ppm Malachite Green | ||
*Large scale PVA-Alg-NaMT no citric acid synthesis | *Large scale PVA-Alg-NaMT no citric acid synthesis |
Revision as of 10:28, 20 February 2015
PVA-Alg Bead Synthesis | <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page <html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html> </html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html> |
February 20, 2015
ProcedureProcedure adapted from | Kuo-Ying Amanda Wu and Keith D. Wisecarver (1992)<br.> <br.> PVA-Alg-NaMT (no citric acid)
MeasurementsNotes |