Procedure detailed by [http://openwetware.org/index.php?title=User:Matt_Hartings/Notebook/AU_Biomaterials_Design_Lab/2014/08/26&action=edit Dr Hartings] | Procedure detailed by [http://openwetware.org/index.php?title=User:Matt_Hartings/Notebook/AU_Biomaterials_Design_Lab/2014/08/26&action=edit Dr Hartings] | ||
*Polymer-10% Clay Film | *Polymer-10% Clay Film | ||
** | **1.0050g PVA and 0.12g sodium montmorillonite (~1g PVA and ~.1g NaM) | ||
*Polymer Film | *Polymer Film | ||
** | **1.0036g PVA (~1g) | ||
====Malachite Green Stock Solutions==== | ====Malachite Green Stock Solutions==== | ||
*2.0ppm | |||
**(2.0ppm)(100mL)=(200.0ppm)*V | |||
**V=1mL of 200.0ppm solution in 99.0mL water | |||
*1.7ppm (25mL) | |||
**(1.7ppm)(25mL)=(8.0ppm)*V | |||
**V=5.31mL of 8.0ppm solution in 19.69mL water | |||
Take UV-vis measurements | |||
<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### --> | <!-- ##### DO NOT edit below this line unless you know what you are doing. ##### --> |
Revision as of 09:48, 29 August 2014
Film Syntheses, Make Stock Solutions | <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page <html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html> </html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html> |
August 29, 2014ProceduresCompleting Film SynthesisContinued from Wednesday, 8/27/2014
Beginning New Film SynthesisProcedure detailed by Dr Hartings
Malachite Green Stock Solutions
Take UV-vis measurements |