Objective

    • Mix pellet, MOF-5 and acetone--> cast and then put through extruder
    • Make filament with ABS and MOF-5 then cut and mix with acetone and cast
    • Make filament with ABS and MOF-5 then melt

Casting

  • Made 5% MOF-5 with ABS and acetone
    • .2523 g MOF-5, 4.7536 g ABS, 30 mL acetone
  • Make ABS filament using filabot, then dope with MOF-5
    • 1.0021g of filament made from this date and dissolved in 10 mL of acetone
  • The results from making the filabot filament, mixing it with the solvent and the MOF-5 then casting it
  • Premadefilament5 19 2014.png