Day 20: Preparing for Electro Deposition

  • Today we made 15 electrodes which we cut and then epoxied after we discovered we only had two samples that were usable so we made more. These new samples were placed inside the oven for 4 hours at 125 degrees. We will electro deposit on Friday with the new samples that we have made.