* Make 50 mL 5 M KNO<sub>3</sub> solution for ionic strength adjustments with silver ion-selective electrode.
+
* Make 50 mL 5 M [http://www.sciencelab.com/msds.php?msdsId=9927232| KNO<sub>3</sub>] solution for ionic strength adjustments with silver ion-selective electrode.
 
* Make LB/agar solution.
 
* Make LB/agar solution.
 
* Make PLA2002D + 5wt% Laponite (PLA + 5LMT) using dichloromethane.
 
* Make PLA2002D + 5wt% Laponite (PLA + 5LMT) using dichloromethane.

Revision as of 12:10, 6 February 2013

<!-- sibboleth --><div id="lncal1" style="border:0px;"><div style="display:none;" id="id">lncal1</div><div style="display:none;" id="dtext"></div><div style="display:none;" id="page">User:Melissa Novy/Notebook/CHEM-572/2013/02/06</div><div style="display:none;" id="fmt">yyyy/MM/dd</div><div style="display:none;" id="css">OWWNB</div><div style="display:none;" id="month"></div><div style="display:none;" id="year"></div><div style="display:none;" id="readonly">Y</div></div>

BDLlogo 300.png <sitesearch>title=Search this Project</sitesearch>

Customize your entry pages <html><img src="/images/a/aa/Help.png" border="0" /></html>

Objectives

  • Make 50 mL 5 M KNO3 solution for ionic strength adjustments with silver ion-selective electrode.
  • Make LB/agar solution.
  • Make PLA2002D + 5wt% Laponite (PLA + 5LMT) using dichloromethane.

Calculations for 5 M KNO3

  MW KNO3: 101.10 g/mol
  0.050 L × 5 M KNO3 = 0.25 mol KNO3
  0.25 mol KNO3 × (101.10 g/1 mol KNO3) = 25.275 g KNO3
  • Actual mass KNO3: 25.2756 g
  • KNO3 was placed in a glass screw-top bottle and 50 mL of pure H2O was added. The solution was stirred and heated at 70°C for 3 hours to dissolve the KNO3.

PLA2002D + 5wt% Laponite Film

  • 1 g of PLA was dissolved in 10 mL of dichloromethane in a fume hood.
  • 0.05 g Laponite was dispersed in 5 mL of dichloromethane, and then added to the PLA solution.
  • The solution was stirred for 1 h and then cast into a Teflon dish.
  • The dish was left under the fume hood to encourage evaporation of the dichloromethane.