|style="background-color: #EEE"|[[Image:owwnotebook_icon.png|128px]]<span style="font-size:22px;"> Project name</span>
|style="background-color: #F2F2F2" align="center"|<html><img src="/images/9/94/Report.png" border="0" /></html> [[{{#sub:{{FULLPAGENAME}}|0|-11}}|Main project page]]<br />{{#if:{{#lnpreventry:{{FULLPAGENAME}}}}|<html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>[[{{#lnpreventry:{{FULLPAGENAME}}}}{{!}}Previous entry]]<html>&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;</html>}}{{#if:{{#lnnextentry:{{FULLPAGENAME}}}}|[[{{#lnnextentry:{{FULLPAGENAME}}}}{{!}}Next entry]]<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html>}}
|style="background-color: #F2F2F2" align="center"|[[File:Report.png|frameless|link={{#sub:{{FULLPAGENAME}}|0|-11}}]][[{{#sub:{{FULLPAGENAME}}|0|-11}}|Main project page]]<br />{{#if:{{#lnpreventry:{{FULLPAGENAME}}}}|[[File:Resultset_previous.png|frameless|link={{#lnpreventry:{{FULLPAGENAME}}}}]][[{{#lnpreventry:{{FULLPAGENAME}}}}{{!}}Previous entry]]&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;}}{{#if:{{#lnnextentry:{{FULLPAGENAME}}}}|[[{{#lnnextentry:{{FULLPAGENAME}}}}{{!}}Next entry]][[File:Resultset_next.png|frameless|link={{#lnnextentry:{{FULLPAGENAME}}}}]]}}
|-
|-
| colspan="2"|
| colspan="2"|
<!-- ##### DO NOT edit above this line unless you know what you are doing. ##### -->
<!-- ##### DO NOT edit above this line unless you know what you are doing. ##### -->
==Entry title==
==PLA Film==
* Insert content here...
* Make Polylactic acid (PLA) film with MOF-5 that was made [[User:Megan L. Channell/Notebook/Masters Research/2013/10/3|here]].


==Protocol==
#0.1 %, 0.5 %, 1.0 %, 5.0 %, 10 % and 0 % w/v.
##0.1 % - 0.9993 g PLA, 0.0013 g MOF-5, 10 mL dichloromethane
##0.5 % - 0.9951 g PLA, 0.0052 g MOF-5, 10 mL dichloromethane
##1.0 % - 0.9904 g PLA, 0.0099 g MOF-5, 10 mL dichloromethane
##5.0 % - 0.9497 g PLA, 0.0495 g MOF-5, 10 mL dichloromethane
##10.0 % - 0.9000 g PLA, 0.9899 g MOF-5, 10 mL dichloromethane 
##0 % - 0.999 g PLA, 10 mL dichloromethane
#Used the ultrasonic to mix each sample in a plastic vial until dissolved completely.
#Once dissolved, poured into molds to set.


==Note==
The 10% is not 10% because there was too much MOF-5.  This needs to be re-done.
<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### -->
<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### -->
|}
|}


__NOTOC__
__NOTOC__

Latest revision as of 23:30, 26 September 2017

Project name Main project page
Previous entry      Next entry

PLA Film

  • Make Polylactic acid (PLA) film with MOF-5 that was made here.

Protocol

  1. 0.1 %, 0.5 %, 1.0 %, 5.0 %, 10 % and 0 % w/v.
    1. 0.1 % - 0.9993 g PLA, 0.0013 g MOF-5, 10 mL dichloromethane
    2. 0.5 % - 0.9951 g PLA, 0.0052 g MOF-5, 10 mL dichloromethane
    3. 1.0 % - 0.9904 g PLA, 0.0099 g MOF-5, 10 mL dichloromethane
    4. 5.0 % - 0.9497 g PLA, 0.0495 g MOF-5, 10 mL dichloromethane
    5. 10.0 % - 0.9000 g PLA, 0.9899 g MOF-5, 10 mL dichloromethane
    6. 0 % - 0.999 g PLA, 10 mL dichloromethane
  2. Used the ultrasonic to mix each sample in a plastic vial until dissolved completely.
  3. Once dissolved, poured into molds to set.

Note

The 10% is not 10% because there was too much MOF-5. This needs to be re-done.