Synthesizing AuNP Fibers Main project page
Previous entry      


Objective

To make 3 solutions of AuNP/BSA protein fibers.

Description

  1. Make 3 solutions with an Au/BSA mole ratio = 166
  2. Combine 1 mL of 3.66 mM HAuCl4 and 1.27 mL of 0.0173 mM BSA in a test tube.
  3. Dilute to 10 mL with water.
  4. Place in oven at 75°C.
  5. Leave solutions in oven for 3.5 hr.

Data

  • AuNP fiber solutions:

Image:Aunp fiber solutions 4-11-12.JPG