User:Jacob Esenther/Notebook/Chem 571/2015/03/03

From OpenWetWare
Jump to navigationJump to search
Biomaterials Design Lab Main project page
Previous entry      Next entry



Objective

  • Check on the status of the GC
  • Create a large amount of gold nanofibers

Description

  1. GC still does not work despite the repair man coming. Darn ...
  2. Gold Nanofibers
    1. The solutions were made with the standard 45:1 Gold:Lysozyme Concentrations
      • 45:1 - 1.40mL of Lysozyme solution, 0.5mL of HAuCl4 solution, and 3.1mL H2O

Data

  • The solutions were made within a viable range as all fibers were formed. 80 5mL samples were made

Notes

Be sure to stretch and warm up your hands before using a pipette on a billion samples. May lead to carpal tunnel.