Line 9: | Line 9: | ||
[[Image:nails ats2.jpg]] | [[Image:nails ats2.jpg]] | ||
*Figure 1. Shows the set up of the modified adhesive strength study. We are hoping that the smaller surface area and longer nail length will lead to usable data. | *Figure 1. Shows the set up of the modified adhesive strength study. We are hoping that the smaller surface area and longer nail length will lead to usable data. | ||
*All of the nails are steel, two are cured with epoxy coating, and two are cured with epoxy and TiO2 coating. | |||
==Thermal energy study with epoxy and TiO2== | ==Thermal energy study with epoxy and TiO2== |
Revision as of 12:11, 6 March 2015
Project name | <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page <html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html> </html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html> |
March 4 - New nail adhesive strength study
Thermal energy study with epoxy and TiO2
Coatings with JA-230
|