==Protocol== | |||
30 % clay solution beads were prepared with the following volumes: | |||
[[Image:Screenshot 2016-09-21 at 11.11.07 AM.png]] | |||
40 % clay solution beads were prepared with the following volumes: | |||
[[Image:Screenshot 2016-09-21 at 11.08.48 AM.png]] | |||
Except for the solution, we followed [http://openwetware.org/wiki/User:Mary_Mendoza/Notebook/CHEM_581:_Experimental_Chemistry_I/2014/11/21 | this protocol] | |||
==Observations== | |||
The beads looked finer and smaller than previous beads. After removing ethylacetate, some of the beads show to have clumped, both for 30 and for 40 percent clay. Additionally, the beads seemed to have a lower density of water: now, the beads form the upper phase of the water - beads layers. | |||
<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### --> | <!-- ##### DO NOT edit below this line unless you know what you are doing. ##### --> |
Revision as of 09:33, 21 September 2016
Project name | <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page <html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html> </html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html> |
Tasklist
Protocol30 % clay solution beads were prepared with the following volumes:
Except for the solution, we followed | this protocol ObservationsThe beads looked finer and smaller than previous beads. After removing ethylacetate, some of the beads show to have clumped, both for 30 and for 40 percent clay. Additionally, the beads seemed to have a lower density of water: now, the beads form the upper phase of the water - beads layers. |