User:Moira M. Esson/Notebook/CHEM-581/2012/11/16
From OpenWetWare
(Difference between revisions)
(→Entry title) |
(→UV-vis porhyrin films) |
||
| Line 11: | Line 11: | ||
#Test swelling on all crosslinked glutaraldehyde films | #Test swelling on all crosslinked glutaraldehyde films | ||
==UV-vis porhyrin films== | ==UV-vis porhyrin films== | ||
| - | + | General protocol for UV-vis on porphyrin films: | |
| - | + | #Remove crosslinked porphyrin films from deionized H<sub>2</sub>O and pat dry using a paper towel | |
| + | #Using a quartz cuvette as a guide, cut a strip of paper the same width as the quartz cuvette. | ||
| + | #Using the strip of paper as a guide and scissors(or a similar sharp instrument) carefully cut the porphyrin film the same width as the paper reference. When cutting the film, try and use a smooth portion of film. | ||
| + | #Measure the thickness of the film. This will be used as the pathlength. | ||
| + | #Using forceps, carefully place the cut strip of film in a clean quartz cuvette. | ||
| + | #Using a spatula, gently press the film against the cuvette. | ||
| + | #Carefully place the cuvette into the UV-vis. | ||
| + | #Measure following the general protocol for | ||
<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### --> | <!-- ##### DO NOT edit below this line unless you know what you are doing. ##### --> | ||
Revision as of 18:55, 26 November 2012
Main project page Previous entry Next entry
| |
Objectives