ObjectiveSamples for group A Make samples using the stock solutions I prepped yesterday.
Make stock solutions of lysozyme and myoglobin for experiments DescriptionSamples for group A Solutions were added to glass test tubes, covered with aluminum foil, and placed in an oven (set to 80°C) for 4 hours. DataStock solutions