User:Keyun Wang/Notebook/Experimental Biological Chemistry I/2013/01/29

From OpenWetWare
Jump to navigationJump to search
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
Experimental Biochemistry II <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page
<html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html>&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;</html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html>

Purpose

  • Start making sample Silver film with proposed protocol

Procedure

  • 3.45g of AgNO3 was weighted out and placed in a 50mL Erylenmeyer flask.
  • 0.8g of Laponite clay was weighted out and placed in same Erlenmeyer flask as above.
  • The 0.8g of Laponite clay was calculated in the following ways:
  Cationic exchange capacity of Laponite: 0.55 milliequivilient/gram
  Weight % of silver to be exchanged in Clay: 95%
  Calculation is shown as follows:
  ___________
  • 10mL of 50/50 water/ethanol solution was made by combining 5mL of water and 5mL of ethanol in a 10mL graduated cylinder.
  • 10mL of water/ethanol solution was poured into Erylenmeyer flask along with a stir bar.
  • The Erylenmeyer flask containing the solution is placed on stir plate for 24 hours.