A new film was synthesized but using a | A new film was synthesized but using a 10% exfoliated clay with a 4% stock. XRD measurements were preformed on previously tested films. Analysis of DSC and UV-Vis data was continued. | ||
==Description== | ==Description== |
Revision as of 12:09, 19 September 2014
Biomaterials Design Lab | <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page <html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html> </html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html> |
ObjectiveA new film was synthesized but using a 10% exfoliated clay with a 4% stock. XRD measurements were preformed on previously tested films. Analysis of DSC and UV-Vis data was continued. Description
DataExfoliated Film
Rerun of the PVA Film Absorption NotesIt is recommended to use acetone to clean the vials after disposing of the Malachite Green H2O. This does not completely clean the vial, whether the residue on the glass makes an impact is still being determined.
|