Objective
Protocol
Use 1.0045g of PVA in 2.7701g NaMT in order to make the 10% clay film. Using the same protocol as August 27th, 2014.
Prepared a PVA-film soaked in 80ppm Malachite Green for XRD analysis. We secured the film to the holder using tape and an XRD of the tape alone has been taken for comparison.
|