Note: These AuNPs will be used in the silica coating procedure. See calculations below.
Note: These AuNPs will be used in the silica coating procedure. See calculations below.
==Calculating amount and concentration of PVP to add to AuNP==
* There must be 60PVP/1nm<sup>2</sup> of AuNP
r= xnm
surface area of a sphere = 4πr<sup>2</sup>
                        = 4π(x x 10<sup>-9</sup>m)<sup>2</sup>
                        = xm<sup>2</sup>
                        = xnm<sup>2</sup>





Revision as of 07:24, 12 June 2013

Project name <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page
<html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html>&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;</html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html>

AuNP synthesis

Note: These AuNPs will be used in the silica coating procedure. See calculations below.

Calculating amount and concentration of PVP to add to AuNP

  • There must be 60PVP/1nm2 of AuNP

r= xnm

surface area of a sphere = 4πr2

                        = 4π(x x 10-9m)2
                        = xm2
                        = xnm2