User:Alexander Cvitan/Notebook/Experimental Biological Chemistry Lab/2014/03/19: Difference between revisions

From OpenWetWare
Jump to navigationJump to search
No edit summary
No edit summary
Line 7: Line 7:
<!-- ##### DO NOT edit above this line unless you know what you are doing. ##### -->
<!-- ##### DO NOT edit above this line unless you know what you are doing. ##### -->
==Objective==
==Objective==
* Synthesize 30:1 lysozyme-AuNP.
* Synthesize more 30:1 lysozyme linked gold nanoparticles.


==Procedure==
==Procedure==

Revision as of 15:34, 17 April 2014

Biomaterials Design Lab: Spring 2014 <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page
<html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html>&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;</html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html>

Objective

  • Synthesize more 30:1 lysozyme linked gold nanoparticles.

Procedure

Creating Stock Solutions of Gold and Lysozyme

  • As seen below, each stock solution was created following the calculations in the table.
  • Each solution was created using a volumetric flask and deionized water.


Synthesizing Lysozyme-AuNPs

  • As seen below, each solutions was created using the following calculations.
  • We made 21 tubes total.