Objective

  • Take 1 mL aliquots of lysozyme-AuNP and BSA-AuNP synthesized yesterday.
  • Centrifuge aliquots and remove supernatant.
  • Retest all treatments with samples of pure fibers.

Procedure

  • 1ml aliquots were prepared for all newly synthesized AuNP's. Lysozyme: 35:1 55:1 110:1 ------- BSA: 100:1
  • All 1ml tubes for the 55:1 and 110:1 ratios were spun down in a centrifuge. Supernatant was removed in order to get pure fibers.
  • To the pure fiber samples chelators, and buffers were added.
  • At this point we ran out of time.